ASTM A514/A514M-05 适用于焊接的高屈服强度淬火和回火合金钢板
1.1 This specification covers quenched and tempered alloy steel plates of structural quality in thicknesses of 6 in. [150 mm] and under intended
Standard Specification for High-Yield-Strength, Quenched and Tempered Alloy Steel Plate, Suitable for Welding
ASTM A514/A514M-00 适用于焊接的高屈服强度淬火和回火合金钢板
1.1 This specification covers quenched and tempered alloy steel plates of structural quality in thicknesses of 6 in. [150 mm] and under intended
Standard Specification for High-Yield-Strength, Quenched and Tempered Alloy Steel Plate, Suitable for Welding
ASTM A514/A514M-05(2009 焊接用经淬火与回火的高屈服强度合金钢板标准规范
1.1 This specification covers quenched and tempered alloy steel plates of structural quality in thicknesses of 6 in. [150 mm
Standard Specification for High-Yield-Strength, Quenched and Tempered Alloy Steel Plate, Suitable for Welding
ASTM A514/A514M-13 焊接用经淬火与回火的高屈服强度合金钢板的标准规格
1.1 This specification covers quenched and tempered alloy steel plates of structural quality
Standard Specification for High-Yield-Strength, Quenched and Tempered Alloy Steel Plate, Suitable for Welding
ASTM A514/A514M-14 焊接用经淬火与回火的高屈服强度合金钢板的标准规格
1.1 This specification covers quenched and tempered alloy steel plates of structural quality
Standard Specification for High-Yield-Strength, Quenched and Tempered Alloy Steel Plate, Suitable for Welding
ASTM A517/A517M-06 压力容器用经回火与淬火的高强度合金钢板
1.1 This specification covers high-strength quenched and tempered alloy steel plates intended for use in fusion welded boilers and other pressure
Standard Specification for Pressure Vessel Plates, Alloy Steel, High-Strength, Quenched and Tempered
ASTM A517/A517M-10 压力容器用经回火与淬火的高强度合金钢板
1.1 This specification covers high-strength quenched and tempered alloy steel plates intended for use in fusion welded boilers
Standard Specification for Pressure Vessel Plates, Alloy Steel, High-Strength, Quenched and Tempered
ASTM A734/A734M-87a(2003 经淬火和回火的合金钢与高强度低合金钢压力容器板的标准规范
1.1 This specification covers quenched-and-tempered alloy steel and high-strength low-alloy steel plates for piping components and welded pressure
Standard Specification for Pressure Vessel Plates, Alloy Steel and High-Strength Low-Alloy Steel, Quenched-and-Tempered
ASTM A734/A734M-87a(1997 经淬火和回火的合金钢与高强度低合金钢压力容器板的标准规范
1.1 This specification covers quenched-and-tempered alloy steel and high-strength low-alloy steel plates for piping components and welded pressure
Standard Specification for Pressure Vessel Plates, Alloy Steel and High-Strength Low-Alloy Steel, Quenched-and-Tempered
ASTM A734/A734M-87a(2007 经淬火和回火的合金钢与高强度低合金钢压力容器板的标准规范
1.1 This specification covers quenched-and-tempered alloy steel and high-strength low-alloy steel plates for piping components
Standard Specification for Pressure Vessel Plates, Alloy Steel and High-Strength Low-Alloy Steel, Quenched-and-Tempered
ASTM A734/A734M-12 经淬火和回火的合金钢与高强度低合金钢压力容器板的标准规格
1.1 This specification covers quenched-and-tempered alloy steel and high-strength low-alloy steel plates for piping components
Standard Specification for Pressure Vessel Plates, Alloy Steel and High-Strength Low-Alloy Steel, Quenched-and-Tempered
AS/NZS 1554.4:2004 结构钢焊接.高强度淬火和回火钢的焊接
Specifies requirements for the welding of steel structures made up of combinations of steel plate, sheet or sections, including hollow sections
Structural steel welding - Welding of high strength quenched and tempered steels
ASTM A852/A852M-01 最小屈服强度为70 Ksi(485 MPa),厚度为4 in(100 mm)的经淬火和回火的低合金结构钢板
1.1 This specification covers quenched and tempered high-strength low-alloy structural steel plates for welded, riveted, or bolted construction
Standard Specification for Quenched and Tempered Low-Alloy Structural Steel Plate with 70 ksi [485 MPa] Minimum Yield Strength to 4 in. [100 mm] Thick
ASTM A852/A852M-00 最小屈服强度为70 Ksi(485 MPa),厚度为4 in(100 mm)的经淬火和回火的低合金结构钢板
1.1 This specification covers quenched and tempered high-strength low-alloy structural steel plates for welded, riveted, or bolted construction
Standard Specification for Quenched and Tempered Low-Alloy Structural Steel Plate with 70 ksi [485 MPa] Minimum Yield Strength to 4 in. [100 mm] Thick
ASTM A852/A852M-03(2007 最小屈服强度为70 Ksi(485 MPa),厚度为4 in(100 mm)的经淬火和回火的低合金结构钢板
1.1 This specification covers quenched and tempered high-strength low-alloy structural steel plates for welded, riveted, or bolted construction
Standard Specification for Quenched and Tempered Low-Alloy Structural Steel Plate with 70 ksi [485 MPa] Minimum Yield Strength to 4 in. [100 mm] Thick
ASTM A514/A514M-05 适用于焊接的高屈服强度淬火和回火合金钢板
1.1 This specification covers quenched and tempered alloy steel plates of structural quality in thicknesses of 6 in. [150 mm] and under intended
Standard Specification for High-Yield-Strength, Quenched and Tempered Alloy Steel Plate, Suitable for Welding
ASTM A514/A514M-00 适用于焊接的高屈服强度淬火和回火合金钢板
1.1 This specification covers quenched and tempered alloy steel plates of structural quality in thicknesses of 6 in. [150 mm] and under intended
Standard Specification for High-Yield-Strength, Quenched and Tempered Alloy Steel Plate, Suitable for Welding
ASTM A514/A514M-05(2009 焊接用经淬火与回火的高屈服强度合金钢板标准规范
1.1 This specification covers quenched and tempered alloy steel plates of structural quality in thicknesses of 6 in. [150 mm
Standard Specification for High-Yield-Strength, Quenched and Tempered Alloy Steel Plate, Suitable for Welding
ASTM A514/A514M-13 焊接用经淬火与回火的高屈服强度合金钢板的标准规格
1.1 This specification covers quenched and tempered alloy steel plates of structural quality
Standard Specification for High-Yield-Strength, Quenched and Tempered Alloy Steel Plate, Suitable for Welding
ASTM A514/A514M-14 焊接用经淬火与回火的高屈服强度合金钢板的标准规格
1.1 This specification covers quenched and tempered alloy steel plates of structural quality
Standard Specification for High-Yield-Strength, Quenched and Tempered Alloy Steel Plate, Suitable for Welding
ASTM A517/A517M-06 压力容器用经回火与淬火的高强度合金钢板
1.1 This specification covers high-strength quenched and tempered alloy steel plates intended for use in fusion welded boilers and other pressure
Standard Specification for Pressure Vessel Plates, Alloy Steel, High-Strength, Quenched and Tempered
ASTM A517/A517M-10 压力容器用经回火与淬火的高强度合金钢板
1.1 This specification covers high-strength quenched and tempered alloy steel plates intended for use in fusion welded boilers
Standard Specification for Pressure Vessel Plates, Alloy Steel, High-Strength, Quenched and Tempered
ASTM A734/A734M-87a(2003 经淬火和回火的合金钢与高强度低合金钢压力容器板的标准规范
1.1 This specification covers quenched-and-tempered alloy steel and high-strength low-alloy steel plates for piping components and welded pressure
Standard Specification for Pressure Vessel Plates, Alloy Steel and High-Strength Low-Alloy Steel, Quenched-and-Tempered
ASTM A734/A734M-87a(1997 经淬火和回火的合金钢与高强度低合金钢压力容器板的标准规范
1.1 This specification covers quenched-and-tempered alloy steel and high-strength low-alloy steel plates for piping components and welded pressure
Standard Specification for Pressure Vessel Plates, Alloy Steel and High-Strength Low-Alloy Steel, Quenched-and-Tempered
ASTM A734/A734M-87a(2007 经淬火和回火的合金钢与高强度低合金钢压力容器板的标准规范
1.1 This specification covers quenched-and-tempered alloy steel and high-strength low-alloy steel plates for piping components
Standard Specification for Pressure Vessel Plates, Alloy Steel and High-Strength Low-Alloy Steel, Quenched-and-Tempered
ASTM A734/A734M-12 经淬火和回火的合金钢与高强度低合金钢压力容器板的标准规格
1.1 This specification covers quenched-and-tempered alloy steel and high-strength low-alloy steel plates for piping components
Standard Specification for Pressure Vessel Plates, Alloy Steel and High-Strength Low-Alloy Steel, Quenched-and-Tempered
AS/NZS 1554.4:2004 结构钢焊接.高强度淬火和回火钢的焊接
Specifies requirements for the welding of steel structures made up of combinations of steel plate, sheet or sections, including hollow sections
Structural steel welding - Welding of high strength quenched and tempered steels
ASTM A852/A852M-01 最小屈服强度为70 Ksi(485 MPa),厚度为4 in(100 mm)的经淬火和回火的低合金结构钢板
1.1 This specification covers quenched and tempered high-strength low-alloy structural steel plates for welded, riveted, or bolted construction
Standard Specification for Quenched and Tempered Low-Alloy Structural Steel Plate with 70 ksi [485 MPa] Minimum Yield Strength to 4 in. [100 mm] Thick
ASTM A852/A852M-00 最小屈服强度为70 Ksi(485 MPa),厚度为4 in(100 mm)的经淬火和回火的低合金结构钢板
1.1 This specification covers quenched and tempered high-strength low-alloy structural steel plates for welded, riveted, or bolted construction
Standard Specification for Quenched and Tempered Low-Alloy Structural Steel Plate with 70 ksi [485 MPa] Minimum Yield Strength to 4 in. [100 mm] Thick
ASTM A852/A852M-03(2007 最小屈服强度为70 Ksi(485 MPa),厚度为4 in(100 mm)的经淬火和回火的低合金结构钢板
1.1 This specification covers quenched and tempered high-strength low-alloy structural steel plates for welded, riveted, or bolted construction
Standard Specification for Quenched and Tempered Low-Alloy Structural Steel Plate with 70 ksi [485 MPa] Minimum Yield Strength to 4 in. [100 mm] Thick
编辑:北检院编辑部